Skip to main content

Table 2 Characterization results of the prepared nanofibers

From: Co-electrospun nanofibrous mats loaded with bitter gourd (Momordica charantia) extract as the wound dressing materials: in vitro and in vivo study

Samples

Contact angle (°)

UTS (MPa)

Porosity (%)

WVP mg/cm2/h

Water uptake ratio (%)

S1

99.11 ± 15.01

4.37 ± 0.90

80.07 ± 6.04

15.95 ± 1.21*

12. 21 ± 1.43

S2

74.76 ± 8.99

2.68 ± 0.05*

79.57 ± 8.26

15.17 ± 2.24*

15.32 ± 2.44

S3

64. 52 ± 11.04*

2.80 ± 0.85*

81.98 ± 5.26

16.01 ± 0.98*

15.98 ± 1.59

S4

22.92 ± 9.01*

1.62 ± 0.50*

75.31 ± 9.31

13. 90 ± 2.43*

20.93 ± 4.03*

Open container

   

31.03 ± 4.22

 
  1. Values represent the mean ± SD, n = 3. *p < 0.05 in comparison with the control group (obtained by one-way ANOVA)